After welding 4130 tubing (for a roll cage), I know a guy, (a very reputable guy) who is dousing it with WD-40. I know you are supposed to anneal a 4130 joint but what does the WD-40 do? He does not anneal the tubing after spraying with WD-40.
Before you say he is doing it wrong, his work stands up to the worst abuse possible. Anyone seen this before?
Before you say he is doing it wrong, his work stands up to the worst abuse possible. Anyone seen this before?