Can anyone tell me what happens to the tensile strength of 3CR12 parent material in the immediate area of a weld.
Does it become normalised. If so, how does this effect the yield stress (normally 320 N/mm^2 min.)
 
Replies continue below

Recommended for you

Martyn,
The welding of 3CR12 causes embrittlement associated with severe grain growth in the heat affected zone and fusion zone. This will lower mechanical properties such as tensile & yield point.