Aug 7, 2006 #1 Bakos Industrial Joined Aug 7, 2006 Messages 2 Location US Greetings and salutations, from the new guy- Question: Does 304SS weld the same as 301SS and can they be welded together? Cheers-
Greetings and salutations, from the new guy- Question: Does 304SS weld the same as 301SS and can they be welded together? Cheers-
Aug 7, 2006 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Without getting into too much detail, I have a homework assignment for you (newbie). Go to the web site below and review information on 301 ss and 304 ss; http://www.aksteel.com/markets_products/stainless_austenitic.asp Upvote 0 Downvote
Without getting into too much detail, I have a homework assignment for you (newbie). Go to the web site below and review information on 301 ss and 304 ss; http://www.aksteel.com/markets_products/stainless_austenitic.asp
Aug 7, 2006 #3 btrueblood Mechanical Joined May 26, 2004 Messages 10,035 Location US metengr, You forgot to tell him to come back and post his results for grading. Upvote 0 Downvote
Aug 8, 2006 Thread starter #4 Bakos Industrial Joined Aug 7, 2006 Messages 2 Location US Dead link...wouldn't load. I'll try it again later. Newbie I am, can't deny it (or hide it for that matter). Your patience is much appreciated. I'll check back in later- Upvote 0 Downvote
Dead link...wouldn't load. I'll try it again later. Newbie I am, can't deny it (or hide it for that matter). Your patience is much appreciated. I'll check back in later-
Aug 8, 2006 1 #5 EdStainless Materials Joined May 20, 2004 Messages 16,373 Location Waukesha WI USA Or, for more detailed welding advise try http://www.outokumpu.com/applications/documents/start.asp = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
Or, for more detailed welding advise try http://www.outokumpu.com/applications/documents/start.asp = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm