This is a low load requirement weld using 309 filler to weld 304/304L to A36. If the weld isn't purged will the resulting "sugar" affect the strength of the joint or is it just a cosmetic problem? Maybe I should also be asking what transformation causes the "sugar"? This is a machine application and welding isn't one of my strong points. Any help will be appreciated.