Fabricating a rectangular frame with light gage structural C-Sections, 45 degree mitered at corners.

AISC 9th TABLE J2.4 lists a minimum fillet for up "To 1/4 inclusive". Is an 1/8" all-around weld to much for 12 ga material?

Thank you ...
 
Replies continue below

Recommended for you

1/8" weld is acceptable with 12 GA material.

DaveAtkins
 
Instead of AWS D1.1, welds shall conform to AWS D1.3 for welding sheet steel.
 
Use the AISI code for cold-formed steel, not the AISC. Note also that because the corners of the studs have a radius, you will be using a flare bevel weld or a flare V weld depending on your connection.
 
12 ga. sheet metal (galvanized) is 0.1084 inches thick. If you are welding a fillet on the cut edge, you cannot use the full leg of a 1/8" fillet (reinforcement not allowed on fillet)
 
I have three questions.

1. Can any of the prequalified joints in D1.3 Sec 3 be used?

2. What will the welding symbol look like?

3. Will the welders be qualified per Sec 4 of D1.3?
 