Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Concrete Masonry Bearing Walls 12" to 8" transition

Status
Not open for further replies.

ingenii

Structural
Joined
Oct 5, 2023
Messages
16
Location
US
I have seen a joist manufacturer recommend stacking two courses of 12" concrete block (bond beam on top with lintel course below) on top of an 8" CMU bearing wall to obtain sufficient wall width to allow joists on either side of the wall to be butted together, in order to make the joist spacing uniform in every bay. Assuming the first two courses of 8" block below the 12" are grouted solid - does this arrangement cause any concern for anyone? The overhang on either side of the wall is only 2". I have checked shear assuming uniform bearing pressure at the joist bearing, although it would likely also work if triangular bearing is assumed.
 
This is the first that I've heard of it.

- I imagine that most of the load gets delivered near the interior of the joist seats.

- This becomes corbel-ish without tie reinforcing.

- For 2" over 16", it's probably ok as a corbel. Light-ish loads.

- Maybe the imbeds wind up inside of the 12" face shells such that the load actually is fully over the 8" wall even with the 2" overhang.

I'm not opposed to it but I'd not be excited about being the first person to do it. So I'd be seeking precedent.
 
Agreed with Kootk about not wanting to be the guinea pig.

Will there be vertical bars at regular intervals in grouted cells that extend all the way up to the top of the 12" block?
 
Why not just beef up the embeds so they can cantilever 2"?

I would be concerned that:

1) You'd load the face shells entirely and probably to very uniformly. Spalling potential.

2) You might pry imbedded anchor, or its grouted cell, right out of the block.

c01.JPG
 
I've seen this overhanging bond beam detail before in some retail strip malls near Seattle. 1970s-1980s construction. But they were wood parallel chord roof trusses spanning ~40'-50' so maybe they needed the extra bearing. And I believe it was an exterior wall with parapet - trusses on one side only. So I'd assume there was rebar continuing through from below. Unknown arrangement of ties. That's the only time I've ever seen the detail in the wild or on paper.

Why not just beef up the embeds so they can cantilever 2"?
SJI wants 1/2" clear from edge of embed to face of CMU in the anti-cantilever direction. OP are your joists steel or wood? I figure steel since you said joists.
 
Thanks to everyone who commented here. I have used a similar detail in the past but only with wood trusses. I am considering using this for long span trusses with a higher end reaction. I have attached the detail I am considering. S-6.0 SECTIONS_001.jpgAs the centroid of the reaction for LH joists is 2" from the end of the joist, the reaction still occurs over the 8" wall. The wall was "flared" to get close to the 6" minimum bearing for LH joists on masonry, though I can go less (down to 4") if the joists are specifically checked for the shorter bearing. Bearing pressure under the plate is less than 300 psi. I am specifying f'm of 2500 psi. I do have rebar continuing from below (there are three floors supported in this manner - the roof is independently supported). I have SDC B. My concern arose after reading test data for bearing failures that indicated that cracking between face shell and web commenced at 50% of ultimate load and that the number of courses of grout did not significantly improve the performance. That made me concerned I could "slice off" my face shell (even though I am far less than 50% of ultimate - but engineers are hardwired to obsess over those things).
 
A few clarifications: the 1/2" SJI criteria is the maximum distance the bearing plate can be inset from the face of the CMU. There is no restriction regarding extension beyond the face of the CMU, but I agree that a long extension creates even higher stress on the face shell - which is what I want to avoid.

The LH joist spans are 30'. I am calling for LH instead of K joists to stiffen the floor against vibration as my slab is very thin due to floor-to-floor restrictions set by the architect.

As for belt and suspenders approach, I have been tossing the idea of #3 shear ties in my head - they won't keep the face shell from spalling but will keep the section intact in the event it does.
 
I'd provide at least several layers of ties under the bearing at a minimum. A little mini-column in the 12" block. Just to keep the thing from blowing apart like you say. 300psi is still pretty high. Maybe look at an embedded grillage beam - WF or HSS maybe, stocky. That sort of creates a hinge for the 18-24" of wall at bearing though.
 
I'd provide at least several layers of ties under the bearing at a minimum. A little mini-column in the 12" block. Just to keep the thing from blowing apart like you say. 300psi is still pretty high. Maybe look at an embedded grillage beam - WF or HSS maybe, stocky. That sort of creates a hinge for the 18-24" of wall at bearing though.
Thank you. The ties I was considering were to wrap the top and bottom bars in the 12" block section. The vertical bars are spaced too far apart and are also in the center of the wall, so tying them is of little benefit to my point of concern.
 
I think I'd just offset the joists a few inches on one side of the wall instead of doing a weird detail. Seems easier than proving this works on paper and then hoping it gets installed and performs as planned.
 
This is the first that I've heard of it.

- I imagine that most of the load gets delivered near the interior of the joist seats.

- This becomes corbel-ish without tie reinforcing.

- For 2" over 16", it's probably ok as a corbel. Light-ish loads.

- Maybe the imbeds wind up inside of the 12" face shells such that the load actually is fully over the 8" wall even with the 2" overhang.

I'm not opposed to it but I'd not be excited about being the first person to do it. So I'd be seeking precedent.
I managed to dig up the old detail I had originally followed. It called for 3 1/2" face shells for the 12" block but the thickest face shell I can find is only 2 1/2"..
 

Attachments

Who on the project team wants to do this? How does placing the joists directly opposite one another on either side of the wall help the project? Chances are this doesn't work out over very much of the floor area anyway because of openings in the slab. Are the joists exposed to view? Is this an architectural thing? I'm with jerseyshore - stagger the bearing locations.
 
You'd load the face shells entirely and probably to very uniformly. Spalling potential.
Then use a BAR 1/2"? Can you bear the joists 'side by side' and just use 8"CMU?
 
Who on the project team wants to do this? How does placing the joists directly opposite one another on either side of the wall help the project? Chances are this doesn't work out over very much of the floor area anyway because of openings in the slab. Are the joists exposed to view? Is this an architectural thing? I'm with jerseyshore - stagger the bearing locations.
The mason actually prefers it as it cuts down time to locate and set bearing plates, one plate for two joists (over 600 joists to set on the job). There are also other project restrictions that force this approach. We are constructing a three story building inside an older historic shell. I am limited in the amount of load I can add to the existing columns/footings. It is so tight that if I moved the joists in one bay 12" away from the column on each floor in every other bay, I will need to underpin 60 footings that are 8 feet deep. If I use this approach at only the column locations and stagger everywhere else, I still need to qualify this concept. Then is no reason not to use it everywhere to make the mason happy.

The geometry has never really concerned me. I know it may look like a corbel but turn my detail upside down and you'll see it resembles an 8" stem wall on a continuous footing. The pressure on the 12" block is uniform, just like the soil pressure on a footing. We don't treat footings under CMU walls as corbels, and narrow footings with projection from the face of the block less than the depth are checked for shear only and unreinforced in the narrow direction. The only difference being the 12" bond beam course is not homogeneous like the concrete footing. It is comprised of grout and a CMU shell. My concern arose after I read test reports on how block fails under bearing loads (the web cracks and separates from the face shell), and that grout did not add substantially to the capacity.

I believe I can resolve my concern (of web splitting in the block under the load) by using 12" solid block below the bond beam course centered on the joists, and shifting the rebar to either side of the joists. Thanks to everyone for their time and input.
 

Attachments

Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top