metengr, thanks for your answer.
Can you please specify more?
Because 09G2S has some different chemical elements than appear at LC1/LC2/LC3, can't they harm the welding?
 
Any good 70-series filler will work. 09G2S is just a Carbon-Manganese steel. Look at the spec for SA-106 pipe.
 