Jun 9, 2018 #1 stan000 Mechanical Joined Jul 31, 2014 Messages 121 Location CA friends FCAW welder qualified using UT,can be used to weld in production. my answer is YES Your opinion please. Regards stan
friends FCAW welder qualified using UT,can be used to weld in production. my answer is YES Your opinion please. Regards stan
Jun 10, 2018 #2 Khaled Saleh Mechanical Joined Jun 1, 2018 Messages 3 Location SY I think the answer is yes Best regards Khaled Saleh https://mechaniclove.com Upvote 0 Downvote
Jun 10, 2018 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US If you are using ASME Section IX, please read QW-304, QW-191.2. Upvote 0 Downvote
Jun 11, 2018 Thread starter #4 stan000 Mechanical Joined Jul 31, 2014 Messages 121 Location CA Thanks. QW 191.2- The ultrasonic examination in for welders and for welding operators may be conducted on test welds in material 1/2" thick or greater. I need minimum thickness 1/2" to qualify welder by u.t. regards Upvote 0 Downvote
Thanks. QW 191.2- The ultrasonic examination in for welders and for welding operators may be conducted on test welds in material 1/2" thick or greater. I need minimum thickness 1/2" to qualify welder by u.t. regards
Jun 11, 2018 #5 DekDee Petroleum Joined Mar 12, 2012 Messages 1,324 Location PH Stan, ASME IX 2017 is now 1/4" (6 mm) minimum for UT Regards, Shane Upvote 0 Downvote
Jun 12, 2018 Thread starter #6 stan000 Mechanical Joined Jul 31, 2014 Messages 121 Location CA thanks. Regards stan Upvote 0 Downvote