Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Welder Qualification to AWS D1.1

Status
Not open for further replies.

Bagman2524

Structural
Jul 14, 2005
707
Looking to find out what it takes to get a welder qualified to D1.1.
Thanks.
 
Replies continue below

Recommended for you

If you just mean how to test, read section 4- Qualification in the latest version of D1.1/D1.1M.

If the welder has limited experience, I would first employ the services of an AWS-certified welding educator to make sure the welder really knows how to weld.

The automotive sector is sometimes less stringent than other industries so I would consider the above as a minimum.
 
Assuming you have a competent welder, there are testing facilities in many areas that can assist you.
 