you can not qualify a welder by RT or UT for GMAW-S and FCAW welding process.

Is that statement is true? If yes why?
 
False...you cannot qualify a welder with GMAW - Short Circuit by RT.
 
What about Fcaw? David
And why? IS there any reason?
 
Qualification of FCAW by RT is allowed. FCAW is globular transfer, not Short Circuit.
Check out the link below.

Link
 
Thanks david👍 really helpful journal
 