"We took a trial on C95800 (NiAlBr) welding qualification in accordance with ASTM A494 S5.2. We conducted the bend test, but the material broke at the HAZ (Heat-Affected Zone). How can we increase the ductility and resolve this issue? Additionally, is it possible to perform a grain size analysis for the casting process? If so, please let me know."

Note Heat treatment process in accordance with ASTM B148 (Annealing)
 