Matlsguy
Materials
- Jun 1, 2006
- 19
Hello,
Probably to no ones surprise we are experiencing problems with welding In 713. Cracks are showing up on xray in the heat affected zone (HAZ)for about half the parts we weld. I'm taking it upon myself to fix this problem. My question is are In 713 alloys more suceptible to Strain Age Cracking or Liquidation Cracking. The ASM Welding Handbook suggests that in these alloys Strain Cracking may be more likely, but we are detecting cracks in xray prior to the post-weld stress relieve heat treatment. Thanks for any info.
Regards,
Matlsguy
Probably to no ones surprise we are experiencing problems with welding In 713. Cracks are showing up on xray in the heat affected zone (HAZ)for about half the parts we weld. I'm taking it upon myself to fix this problem. My question is are In 713 alloys more suceptible to Strain Age Cracking or Liquidation Cracking. The ASM Welding Handbook suggests that in these alloys Strain Cracking may be more likely, but we are detecting cracks in xray prior to the post-weld stress relieve heat treatment. Thanks for any info.
Regards,
Matlsguy