I'm attaching a 1-1/4 steel plate to a 3/4" steel backing plate. I can use a fillet weld on either side of the 1-1/4" steel plate or use a prepared weld. Does the AISC or AWS have a guide to the minimum fillet weld that should be used based on the plate thickness? and/or is it less costly to use a prepared weld (groove) instead of two large fillet welds?