Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Weld Symbol

Status
Not open for further replies.

Egnorant

Structural
Aug 14, 2012
16
I am welding two plates that are at right angle to each other as shown on the attached. I am not sure how to show the groove weld symbol. Could somebody check whether the symbols shown are correct. I want the welded edge on the right hand side to be flushed/smooth by grinding. Thanks

W2_rkwnui.jpg
 
Replies continue below

Recommended for you

I think what you show works, but I think instead of a G, dont you just draw a horizontal line for flush?
 
Without looking it up, I believe the horizontal line is for flush and the G is for grind smooth.
 
My personal opinion, but I'd be inclined to show a top view and call the welds out there.

Please note that is a "v" (as in Violin) not a "y".
 