Good afternoon all,
A LH2 pressure vessel that was manufactured about 20 years ago was recently opened and had an internal inspection performed. During the inspection, it was discovered that there was incomplete penetration on the nozzle weld, and after referring to the ASME Code, the nozzle did not have to have RT performed at the time of construction.
Does this weld need to be repaired according to NBIC standards or another national standard? What other options are available to ensure continued and safe operation?
Thank you very much
A LH2 pressure vessel that was manufactured about 20 years ago was recently opened and had an internal inspection performed. During the inspection, it was discovered that there was incomplete penetration on the nozzle weld, and after referring to the ASME Code, the nozzle did not have to have RT performed at the time of construction.
Does this weld need to be repaired according to NBIC standards or another national standard? What other options are available to ensure continued and safe operation?
Thank you very much