Hi!
I am looking for some advice regarding the approval range of a WPQR we have, relating to a certain joint fit up.
We have a nozzle 1" Sch 80 4.55mm thick, this is being welded to a flange which is drilled to the internal bore of the 1" pipe. Our weld procedure is qualified upto around 8mm thick.
The thickness of the flange is 50mm thick, our weld thickness is is 4,55mm thick with some re-inforcement, will our weld procedue cover this set up?
I would call the fit up a tee joint
I am looking for some advice regarding the approval range of a WPQR we have, relating to a certain joint fit up.
We have a nozzle 1" Sch 80 4.55mm thick, this is being welded to a flange which is drilled to the internal bore of the 1" pipe. Our weld procedure is qualified upto around 8mm thick.
The thickness of the flange is 50mm thick, our weld thickness is is 4,55mm thick with some re-inforcement, will our weld procedue cover this set up?
I would call the fit up a tee joint