Dear welding experts,
we are manufacturing longitudinal saw weld pipes of api 5l
weld groove: double v(internal saw and external saw)
recently we have weld 50 nos(12.2Meter length)of pipe of size dia.32"Xthi.39mm
we have done 100% Rt of each pipe & results no any porosity found. but after few days we have weld pipe size dia24"Xthi.38mm & rt results found porosity in every pipes.
both pipe size grade(Api 5l x-65) is same, joint geometry is same, saw welding consumables is same,same preheating temp and also we are taking extra care like cleaning of pipe , heating of flux in pipe size 24"X38mm.
then why porosity come in pipe size 24"x38mm in internal saw welding
we are manufacturing longitudinal saw weld pipes of api 5l
weld groove: double v(internal saw and external saw)
recently we have weld 50 nos(12.2Meter length)of pipe of size dia.32"Xthi.39mm
we have done 100% Rt of each pipe & results no any porosity found. but after few days we have weld pipe size dia24"Xthi.38mm & rt results found porosity in every pipes.
both pipe size grade(Api 5l x-65) is same, joint geometry is same, saw welding consumables is same,same preheating temp and also we are taking extra care like cleaning of pipe , heating of flux in pipe size 24"X38mm.
then why porosity come in pipe size 24"x38mm in internal saw welding