I know this is probably too broad a question but any thoughts are helpful.
Are there any guidlines/standards for acceptable weld penetration?
I realize material type, weld wire, etc. do contribute.
For instance I have a drawing with a 3/16 bevel weld that states "welds must penetrate amd adhere to both pieces".
Is there any way to be more specific about weld penetration?
Thanks
AirRider
Are there any guidlines/standards for acceptable weld penetration?
I realize material type, weld wire, etc. do contribute.
For instance I have a drawing with a 3/16 bevel weld that states "welds must penetrate amd adhere to both pieces".
Is there any way to be more specific about weld penetration?
Thanks