We have to do weld build up on SA-216 WCB valve body.Valve is of 600 Rating and size is NPS 8.Maximum depth of the build up is 5 mm.
What are the special precautions to take like preheating or post heating (PWHT is not a Code requirement in this case).Code of construction is ASME B31.1. We shall use GTAW with ER 70S-3
Would you please suggest better wire than ER 70S-3?
We have done without preheating with ER 70S-3 but welding is found cracking.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
What are the special precautions to take like preheating or post heating (PWHT is not a Code requirement in this case).Code of construction is ASME B31.1. We shall use GTAW with ER 70S-3
Would you please suggest better wire than ER 70S-3?
We have done without preheating with ER 70S-3 but welding is found cracking.
Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN