In view of this discussion I have an example of which Im not certain if it contains a B31.3 designated weld defect. Could anyone indicate if there's a weld defect in attached picture, and when applicable which type?
I cant find any real good example of non-acceptance acc to the criteria of the referenced topic, nor acc fig 341.3.2, keeping in mind the required weld metal thickness has to be 10S (see below).
The weld end of the 2 fittings welded in the picture were counterbored on the inside from 40S to 10S. The fittings have been welded without any root gap. There was no external or internal misalignment during welding.
The welds are already RT examined & accepted under B31.3 critieria. Code of construction = B31.3.
I cant find any real good example of non-acceptance acc to the criteria of the referenced topic, nor acc fig 341.3.2, keeping in mind the required weld metal thickness has to be 10S (see below).
The weld end of the 2 fittings welded in the picture were counterbored on the inside from 40S to 10S. The fittings have been welded without any root gap. There was no external or internal misalignment during welding.
The welds are already RT examined & accepted under B31.3 critieria. Code of construction = B31.3.