shaneelliss
Structural
In the plant where I work we have large vehicles that move heavy vats of product around. The vehicles have hard solid tires. The pair of wheels in the front are located together in the center of the machine and rotate to do all the steering and drive the machine. But the front wheels rotate such that it operates similar to a forklift steering where the machine can make a complete circle with nearly a zero foot radius on the back wheel. The vehicles travel on elevated concrete floors. The concrete is always falling apart, ruts develop on the top surface and concrete spalls off the bottom surface. The spalling on the underside is probably due to inadequate design as the rebar is epoxy coated and looks to be in good condition, so it isn't a rust issue. I am guessing the issue at the top is just crushing from wheels traveling and pivoting over time. But the ruts create more dynamic loads on the slab and overtime the slab breaks all the way through with concrete falling out the bottom. It might just be shear failure from the get go, but I can't tell.
The loads on the front axle are 53 kips (static) and on the rear axle are 65 kips (static). The tires are about 16" wide and the imprint appears to be about 12" long on the rear tires and 6" long on the front.
I need to replace sections of the floor that have failed. The plant process makes it really hard to replace sections of floor without shutting down production, which just isn't allowed for any long period of time. I might get three or four days, maybe up to a week if I am lucky. I can try to design the slab for greater shear and bending strength, but I was trying to think of ways to reduce the top surface wear to keep it smoother and reduce the dynamic loads a bit that happen when the floor looses its smoothness. And I need to come up with a way to construct it quickly.
One thought I had was to use precast concrete panels with a steel plate on top, cast into the panels. Anyone have any thoughts on this? It might add that this is in a very corrosive salt environment.
The loads on the front axle are 53 kips (static) and on the rear axle are 65 kips (static). The tires are about 16" wide and the imprint appears to be about 12" long on the rear tires and 6" long on the front.
I need to replace sections of the floor that have failed. The plant process makes it really hard to replace sections of floor without shutting down production, which just isn't allowed for any long period of time. I might get three or four days, maybe up to a week if I am lucky. I can try to design the slab for greater shear and bending strength, but I was trying to think of ways to reduce the top surface wear to keep it smoother and reduce the dynamic loads a bit that happen when the floor looses its smoothness. And I need to come up with a way to construct it quickly.
One thought I had was to use precast concrete panels with a steel plate on top, cast into the panels. Anyone have any thoughts on this? It might add that this is in a very corrosive salt environment.