Can a supplier change the end connection on a valve? without consent from OEM?
I have a 8" Grove valve whose MTR's say it is WE X RF from OEM, where as the actual valve is WE X WE , the supplier says flanged end was cut off and machined to make it a WE, so my question is does this affect the integrity of the valve?
do we have a procedure that specifies how this should be done?
Always be a Student
I have a 8" Grove valve whose MTR's say it is WE X RF from OEM, where as the actual valve is WE X WE , the supplier says flanged end was cut off and machined to make it a WE, so my question is does this affect the integrity of the valve?
do we have a procedure that specifies how this should be done?