RAJMETALLURGY
Materials
WCB with Normalized (940 Deg C) & Tempered (640 Deg C) are getting failure with lower yield and lower UTS. Please guide me to resolve it.
Similarly in the case of Inconel 825 (CU5MCuC) getting failure in elongation (Solution annealed 1900 Deg C & Stabilized @ 960 Deg C). How to solve it, the fracture surface looks like brittle fracture no appearance of cup & Cone.
And is it required to add Ti & Al in the case of Carbon Steel (WCB, LCB) & Low alloy steels (WC6, WC9 & C5). Because am not getting toughness value @-10 deg C. If I stopper am getting good values in +20, +10, 0 Deg but in -10 Deg am not getting more than 27 Joules.
Please help me.
Similarly in the case of Inconel 825 (CU5MCuC) getting failure in elongation (Solution annealed 1900 Deg C & Stabilized @ 960 Deg C). How to solve it, the fracture surface looks like brittle fracture no appearance of cup & Cone.
And is it required to add Ti & Al in the case of Carbon Steel (WCB, LCB) & Low alloy steels (WC6, WC9 & C5). Because am not getting toughness value @-10 deg C. If I stopper am getting good values in +20, +10, 0 Deg but in -10 Deg am not getting more than 27 Joules.