Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Warping Equations for U-Shape

Status
Not open for further replies.

EngDM

Structural
Aug 10, 2021
760
Does anyone have readily available equations for warping and torsional constants for a U-Shape? Would I be okay to use the C-Shape equations? I'm analyzing cold formed U-members for a joist web, and the supplier does not provide these values but I need them to find Feyz as specified in S16 Clause 13.3.2.
 
Replies continue below

Recommended for you

This is the best I have
 

Attachments

  • CISC Torsional Properties.pdf
    248.6 KB · Views: 13
Unless I was going to be doing a whole lot of this, I would just treat the shape as though it were only the two opposing sides acting in strong axis flexure independently. That's where all of the torsional stiffness will be anyhow.

c01.JPG
 
I'm just trying to calculate web compressive strength of Canam Joists. I have a paper from them with most properties except for warping and torsion. I don't think these failure modes would govern a joist anyways considering the ends are sandwiched between the top chords, but best to check
 
Yeah, with short lengths and rotational restraint at each end, it won't take much to prove that torsional buckling won't govern. Probably why the torsion parameters aren't tabulated. With that in mind, I like my poor boy approach even better.
 