Hi,
Is there a formula or rule of thumb that I can use for MIG welding to determing the minimum amount of material required to weld, to avoid burn through?
For example, I want to weld a T-joint. The material thickness is 2mm and the height of the tab to be welded to the base is 6mm. The weld has a 3mm throat and is 10mm long. Will it burn through? What height do I need to have to avoid burn through?
| } 6mm tall
| }
--------
Thanks,
Jeff
Is there a formula or rule of thumb that I can use for MIG welding to determing the minimum amount of material required to weld, to avoid burn through?
For example, I want to weld a T-joint. The material thickness is 2mm and the height of the tab to be welded to the base is 6mm. The weld has a 3mm throat and is 10mm long. Will it burn through? What height do I need to have to avoid burn through?
| } 6mm tall
| }
--------
Thanks,
Jeff