Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Voltage Rating of Kraft Transformer Insulating Paper vs Kraft Diamond Epoxy Paper 1

Status
Not open for further replies.

VLFit

Electrical
Joined
Feb 28, 2005
Messages
120
Location
US
In terms of volts/mil, are these two equal in their voltage ratings. When oil soaked following a full vpi and when not soaked.
 
I haven't heard of kraft diamond paper but I guess it's this

Clicking specs at the bottom of that page, shows 50 kV/mm oil soaked for that product.

I don't think the phrase vacuum pressure impregnation (VPI) applies to any of this, but I gather you mean filling with oil under a vacuum.
 
No difference in KV/mm between the two. BDV in oil is approximately 5-7 times more than in air.
 