5
Dear all,

new to the forum, so please forgive me if i am missing some information.

I am looking for some way to model a tensile test of a polymer (displacement controlled). This, in a second stage, should be used to simulate some microstructure. I have already the parametrization for particles as well as the interface. "Only" the matrix is remaining.

By now i have a simple elastic-plastic model, that can capture the curve of the tensile test. See attached image (purple line: elastic-plastic material curve for Abaqus, blue line: original tensile test curve, blue dots: measured curve in Abaqus). good match i would say. However, the plastic input data needs a bump (stress decrease) after the yield point to capture the behavior of the test data. That's bump is not reasonable to me, as, to my understanding, the plastic curve should be monotonic. But if keep the plastic curve monotonic i always get sth like the red curve. This is understandable, because from the materials side there is some kind of stress relaxation involved, that causes the concave shape of the curve.

As i understand from literature state of the art would be some nonlinear viscoelastic material model like parallel rheological framework. I didn't try parametrizing yet, but i don't see why it should not work (maybe running into overfitting as i have only one tensile test data). But the issue is, that i need some damage model for the second stage when simulating the microstructure. Up to now my data would work nicely with the standard ductile damage model, including triaxiality. But ductile damage does not work with the viscoelastic material model nor creep model.

So, the question is, is there some material model, that can capture this visoelastic effect or generally stress relaxation that does work with ductile damage?

Or the other way round, is there some other damage model (including triaxiality) that works with viscoelastic material models?

kind regards
Wolfgang
 

Attachments

  • MatLaw_TensileTest.png
    MatLaw_TensileTest.png
    119 KB · Views: 3
Last edited:
Replies continue below

Recommended for you

then with displacement controlled tests, you will see load drops in the response curve which will not show up in a load controlled curve. these load drops are an artifice of the displacement controlled loading, as when there is a stiffness drop (due to damage, etc) there will be a load drop and load recovery as displacement increases. whereas most real life loading is effectively load controlled, and when there is a stiffness drop then the response curve shows a horizontal displacement jump at the same load. you have to sort out which behavior represents your reality and make appropriate adjustments to the measured curve.
 
exactly. With load-controlled tests, there might be a rate change in the resulting displacement curve (depending on the load rate).
And that's why i am asking here if sb with expert knowledge knows a solution/approach on how to include these viscoelastic-/plastic effects while maintaining the possibility for damage modelling. Otherwise, I will simply stay with elastic-plastic where i can go into damage modelling.
 
As i understand from literature state of the art would be some nonlinear viscoelastic material model like parallel rheological framework. I didn't try parametrizing yet, but i don't see why it should not work (maybe running into overfitting as i have only one tensile test data). But the issue is, that i need some damage model for the second stage when simulating the microstructure. Up to now my data would work nicely with the standard ductile damage model, including triaxiality. But ductile damage does not work with the viscoelastic material model nor creep model.
According to the "Damage Initiation for Ductile Metals" documentation chapter, ductile damage can be used with PRF and permanent set for rubber-like materials.
 
According to the "Damage Initiation for Ductile Metals" documentation chapter, ductile damage can be used with PRF and permanent set for rubber-like materials.
Thank you very much for your response. Could you provide a link to the documentation? Or maybe which Abaqus Version you are referring to?

My Abaqus 2025 needs Hyperelastic for viscoelastic PRF, but Hyperelastic does interfere with ductile damage, see attached screenshots (Parameters are not correct, just for (i think it was) PEEK from some online source). As PRF cannot be entered from CAE i added it via model -> edit Keywords, see second screenshot

Regards
Wolfgang
 

Attachments

  • 4.png
    4.png
    21.1 KB · Views: 2
  • 3.png
    3.png
    24.9 KB · Views: 2
  • 2.png
    2.png
    24.8 KB · Views: 2
  • 1.png
    1.png
    34.9 KB · Views: 2
I'm using the documentation for Abaqus 2025. It can be accessed only via 3DPassport account but anyone can access it. This is only mentioned once in the chapter "Damage Initiation for Ductile Metals":

The material damage initiation capability for ductile metals:
  • ...
  • can be used with models defined using the parallel rheological framework (ductile, shear, and Hosford-Coulomb criteria, and in Abaqus/Explicit the Johnson-Cook criterion).
If it doesn't work this way (which is understandable considering the individual limitations of these models), you may have to resort to (V)UMAT subroutine. Possibly based on some research papers on the subject.
 