Hi!

I wonder what will happen to pretensioned precast spandrels, whose dimensions are 10ft long (simple span), 8ft tall and 8in thick.
Should I ignore all prestressing forces?
(Like 22 strands with 16kips pullout per each strand.)

Thanks!
 
Replies continue below

Recommended for you

You would likely lose a lot of your stressing for such members unless they were cast in a bed and sawcut to length. Can you use regular reinforcing?

Dik
 
Sounds like a deep beam to me.

And a deep beam requires that the bottom steel be fully developed at the end supports. Not sure how you could do this with pre-tensioned strand. You would need bottom reinforcement with development length extending from the end if it is cast in!
 