Oct 20, 2015 #1 engineer54 Mechanical Joined Jul 14, 2013 Messages 26 Location US Has anyone had any problems using vegetable oil as a rust preventative in a pressure vessel with hydrocarbon liquids?
Has anyone had any problems using vegetable oil as a rust preventative in a pressure vessel with hydrocarbon liquids?
Oct 20, 2015 #2 EdStainless Materials Joined May 20, 2004 Messages 16,369 Location Waukesha WI USA Yes, it doesn't work. Some veg oils dry, some don't, and all of them will be somewhat hydroscopic. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
Yes, it doesn't work. Some veg oils dry, some don't, and all of them will be somewhat hydroscopic. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Oct 20, 2015 Thread starter #3 engineer54 Mechanical Joined Jul 14, 2013 Messages 26 Location US Will the veg oil have any reaction to the hydrocarbon liquids? Upvote 0 Downvote
Oct 21, 2015 #4 mbt22 Chemical Joined Mar 9, 2006 Messages 180 Location GB Depends on the hydrocarbon, some will. Matt Upvote 0 Downvote