Has anyone had any problems using vegetable oil as a rust preventative in a pressure vessel with hydrocarbon liquids?
 
Replies continue below

Recommended for you

Yes, it doesn't work.
Some veg oils dry, some don't, and all of them will be somewhat hydroscopic.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Will the veg oil have any reaction to the hydrocarbon liquids?
 
Depends on the hydrocarbon, some will.

Matt
 