Can anyone give me a best estimate on what material is used to fabricate the pneumatic air motor vane, shown in the photo attached?

As can be seen, it has a slight orange color and appears to be slightly fiberous.

I would like to find a material source and understand how to mold and/or machine components similar to this vane.

thanks in advance for your interest and help
 
My best guess is glass fiber-reinforced phenolic.

Can't help with the other questions.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
I'm familiar with the vanes but don't know the exact material. It is probably a phenolic resin with cotton fabric in it. It is not glass as glass is very abrasive. Several companies matufacture sheets of composites like this and you can buy it from McMaster-Carr.
 
Compositepro,
I will check out a sample from mcmaster to test. Thanks for the reference.
 
Or you can look up the properties of most materials free at
There is not any memory with less satisfaction than the memory of some temptation we resisted.