nickypaliwal
Materials
I have observed our client has used valves with CS body and Duplex SS/SDSS/Alloy 825 trim. Generally manufacturers may recommend DSS/SDSS/ALloy 825 etc grades for valve trim incase they need more strength or torque however from corrosion stand point, can it be justifies using such valves?