Apr 19, 2013 #1 glade Mechanical Joined Jan 28, 2010 Messages 11 Location MY Dear expert what is the different between CS WCB and CS WCC valve material?
Apr 19, 2013 #2 reverman Mechanical Joined Jul 22, 2008 Messages 142 Location US Chemically WCC allows a little more manganese and a little less carbon, Mechanically WCC has a higher minimum yield strength which is why the PT ratings for WCC are slightly higher for WCC when compared to WCB Upvote 0 Downvote
Chemically WCC allows a little more manganese and a little less carbon, Mechanically WCC has a higher minimum yield strength which is why the PT ratings for WCC are slightly higher for WCC when compared to WCB