Dear expert
what is the different between CS WCB and CS WCC valve material?
 
Chemically WCC allows a little more manganese and a little less carbon, Mechanically WCC has a higher minimum yield strength which is why the PT ratings for WCC are slightly higher for WCC when compared to WCB
 