What is valqua number in gasket and from where I can get the complete list of Valqua numbers and its description?
 
I have the the same question. It appears that Valqua is a gasket manufaturer and they number their gasket types with product codes such as #6500=nonasbestos sheet, #7010= virgin PTFE, #133 = asbestos coil packing, etc.

I suggest contacting the HQ for the company at for product brochures or clarification about specific numbers.

Tommy Clifford
Struthers Industries Inc.
 