As I understand the rules, the ASME piping code only permits materials that meet the steel-making requirements of ASTM specifications.
I believe that your vacuum requirement is indirectly necessary in order to produce steels to ASTM requirements
Only "fully killed" carbon steels (e.g. ASTM A106 - GrB)are permitted in certain applications.