Hi!
I would like to know if someone can help me. I would like to hardened material AISI 9260 H (DIN : 65 Si 7) in vakuum furnace. I have some knives with thicknes of 15 mm.Required hardness ofter hardening : 59 - 60 HRC.In the furnace I can get pressure : 8,5 bars.
Best regards
I would like to know if someone can help me. I would like to hardened material AISI 9260 H (DIN : 65 Si 7) in vakuum furnace. I have some knives with thicknes of 15 mm.Required hardness ofter hardening : 59 - 60 HRC.In the furnace I can get pressure : 8,5 bars.