What is the type and composition?

Ref: page 16, April 5, 2012 MACHINE DESIGN magazine. Ace Controls miniature shocks.
just curious.

Thanks

Design for RELIABILITY, manufacturability, and maintainability
 
Replies continue below

Recommended for you

V4A usually refers an austenitic SS that has Mo in it, similar to 316.

= = = = = = = = = = = = = = = = = = = =