Jul 6, 2012 #1 metman Materials Joined Feb 18, 2002 Messages 1,187 Location US What is the type and composition? Ref: page 16, April 5, 2012 MACHINE DESIGN magazine. Ace Controls miniature shocks. just curious. Thanks Design for RELIABILITY, manufacturability, and maintainability
What is the type and composition? Ref: page 16, April 5, 2012 MACHINE DESIGN magazine. Ace Controls miniature shocks. just curious. Thanks Design for RELIABILITY, manufacturability, and maintainability
Jul 6, 2012 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US http://www.google.com/url?sa=t&rct=...mRl07ntpEUVYRNI7g&sig2=v1RRj347XrSGEl0PswTsuQ Upvote 0 Downvote
Jul 7, 2012 #3 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA V4A usually refers an austenitic SS that has Mo in it, similar to 316. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
V4A usually refers an austenitic SS that has Mo in it, similar to 316. = = = = = = = = = = = = = = = = = = = = Plymouth Tube