Jul 10, 2017 #1 212197 Mechanical Joined Jun 2, 2007 Messages 124 Location IN as per UW-11(C),no RT is required for external pressure vessel. What's the rationale?
Jul 10, 2017 #2 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,863 Location US Weld seams are generally in compression. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
Weld seams are generally in compression. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand