Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

UV effects on polyurethane

Status
Not open for further replies.

Gijom

Mechanical
Joined
Jul 24, 2003
Messages
2
Location
FR
I am looking for information of effects on a polyrethane product due to UV exposure (sun exposure)
- aging effect
- degradation (visible or not)
- loose of characteristics
- etc..

Does the type of polyurethane be a parameter ?
 
Yes
I don't know the details of the top of my head, but some chemical types of PU are much more inherenty UV stable than others.

Companies like Bayer or BASF should be able to provide full details.

I can search some old files if really necessary

Regards
pat
 
Pat,

Thanks for your input. I am looking to documents about UV effect on driving belts polyurethane jacket with steel cords inside (looking like the ones used to drive a starter or an alternator in the car)

Any information may help.

Thanks in advance

Gijom
 
yes hddp is sesptable to uv if you put a uv stab. in the mix it will cut down on uv degrgation
 
Compare to other diene elastomers , Polyurethanes show good weathering properties. However the show slight embritlement under sun after years of exposure. It depends on weather conditions (ozone, oxigen sun) and PU type:Polyether based slightly more resistant than polyester based


 