WE HAVE A VESSEL. SHELL QUALITY IS SA333 GR 6. NOZZLE IS SA333 GR6. REINFOREMENT PAD IS SA516 GR 70.
UTS AT ROOM TEMPERATURE (ACTUAL) - 471 MPA AGAINST REQUIRED 486 MPA.
YS AT ROOM TEMPERATURE (ACTUAL) - 306 MPA AGAINST REQUIRED 260 MPA.
REINFORECEMENT PAD CALCULATION AS PER ASME UG-37 DOES NOT INVOLVE UTS.
MY CLIENT WANTS JUSTIFICATION FOR ACCEPTANCE OF THE DEVIATION IN UTS.
WHAT BASIS COULD WE PROVIDE ? WE CAN NOT REJECT THE MATERIAL.
UTS AT ROOM TEMPERATURE (ACTUAL) - 471 MPA AGAINST REQUIRED 486 MPA.
YS AT ROOM TEMPERATURE (ACTUAL) - 306 MPA AGAINST REQUIRED 260 MPA.
REINFORECEMENT PAD CALCULATION AS PER ASME UG-37 DOES NOT INVOLVE UTS.
MY CLIENT WANTS JUSTIFICATION FOR ACCEPTANCE OF THE DEVIATION IN UTS.
WHAT BASIS COULD WE PROVIDE ? WE CAN NOT REJECT THE MATERIAL.