welda
Structural
- Oct 27, 2008
- 2
I am required to UT 316L Stainless penetrators into a vessel body of 30mm thick P355J2 (50D) material. I have used a 309 filler wire. I have welded a calibration block but can't get an echo through the weld material. Does anyone have any experience they would be kind enough to share?