Building piping to ASME B31.3. Client spec requires that all branch connections have 100% MPI and 10% UT. Have tried a specification deviation to allow only MPI which was approved but only for piping with wall thickness less then 3/8".
Had a stub-on "Straight piece of pipe beveled end full pen weld" fail UT now as code calls I am require to have two tracers.Weld failed for incomplete penetration.
Now here is where I'm running into issues.
Only other branch type welds this welder has complete is one stub on some make as failed weld and olets.
The one stub on has a massive re-pad currently welded on top of it. After speaking with NDT contractor they claim that this weld can not be UT.
Now as for the olets (These sit up top of the pipe with a diagonal full pen from the olet to the hole cut into the main run of piping. Current UT guy claims these can not be inspected but means of UT. So as it stands right now i'm hooped for tracers and client does require inspection on olets.
Now my question would be is UT on olets actually possible or am I dealing with a poor technician?
Reason I ask this was 5 months ago on a different job same type of olets same NDT company just a different office had no issue performing UT these olets with a straight beam looking for IP which is about all you will be able to see. We were actually receiving reports stating accept or reject on these welds with identical geometry. So are these reports actually legit? Someone here is giving us false information
Anyone had any experience with this?
Had a stub-on "Straight piece of pipe beveled end full pen weld" fail UT now as code calls I am require to have two tracers.Weld failed for incomplete penetration.
Now here is where I'm running into issues.
Only other branch type welds this welder has complete is one stub on some make as failed weld and olets.
The one stub on has a massive re-pad currently welded on top of it. After speaking with NDT contractor they claim that this weld can not be UT.
Now as for the olets (These sit up top of the pipe with a diagonal full pen from the olet to the hole cut into the main run of piping. Current UT guy claims these can not be inspected but means of UT. So as it stands right now i'm hooped for tracers and client does require inspection on olets.
Now my question would be is UT on olets actually possible or am I dealing with a poor technician?
Reason I ask this was 5 months ago on a different job same type of olets same NDT company just a different office had no issue performing UT these olets with a straight beam looking for IP which is about all you will be able to see. We were actually receiving reports stating accept or reject on these welds with identical geometry. So are these reports actually legit? Someone here is giving us false information
Anyone had any experience with this?