Dear fellow engineers,

So we need to verify anomalies from MFL inspection with UT C-scan on a pipeline.
The model for UT C-scan we used is Olympus Omniscan MX 2. Probe size A12 and scanner speed is 60mm/s.

The range of the MFL anomalies (internal corrosion), approximately a dozen of them are within 10-330mm in width, 19-146mm in length across the pipe, and peak depth of 16-48%.

However, UT C-Scan only get 17% loss at the expected area

My questions are:
1. Any possible limitations on the UT C-scan?
2. Any suggestions to verify the findings? It is believed that C-scan is the best method available to verify internal corrosion.

Thank you.
 
 https://files.engineering.com/getfile.aspx?folder=51d20414-0675-4bfd-997b-55407d2c75cf&file=Capture.JPG
Both inspection methods will have a reliability profile. Decision making with respect to results needs to incorporate the knowledge of those reliability profiles. The method selection process should have documented these profiles.

Have a look at NACE Corrosion 2014, Paper 4139 and


Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Dear Adib CJ,

What's better than to cut the pipes and satisfy thy eyes?

Regards.

DHURJATI SEN
Kolkata, India

 
As you already knew MFL is a Screening tool and it has a lot of limitations eg. pipeline cleanliness, a sensor to wall distance, magnetic interference etc. which can make the data deviation. if all UT parameters are set correctly, it will give you a more accurate result better than the MFL result.
 