Dear All;

Can anyone tell me, whether UT crawler could be used to measure the thickness of 2205 Duplex steel surface?
Thanks in advance

 
Why not?
Use the correct ref stds.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 