I have a remote client who's asking if they can use some old rebar they have on site for one of my designs. Based on the pictures and tags they sent over, it appears that the rebar has been sitting at their site for nearly a decade. I haven't had a chance to inspect it closely, but as you would expect, the photos appear to show pretty rusty surface conditions.
Any opinions on the use of rebar this old? Assume (conservatively) 10% material loss and increase the As (liberally) by... 20%? Any concerns regarding development and lap lengths due to corroded deformations?
As always, any and all opinions are appreciated.
Any opinions on the use of rebar this old? Assume (conservatively) 10% material loss and increase the As (liberally) by... 20%? Any concerns regarding development and lap lengths due to corroded deformations?
As always, any and all opinions are appreciated.