Kindly advise on subjected query if ASTM A234 swaged nipple is used instead of ASTM A105. Is there any major difference/impact ?

Thanks.
 
It would have to be SA 234 WPC versus WPB for a substitution to ensure equal or higher allowable stress values in comparison to SA 105. Other than that read the material specifications on your own.
 
We just plain don't use swage nipples, because we find that when we order them, they're either not in stock or are machined out of barstock...
 