Hi everybody.
Have you used this steel or do you know which grade is or typical use?
Yes, It's look like AISI Serie 61xx, Cr-V Steel (like the legend in some handtool), but i'm not sure about the Moly content in this serie.
C = 0.22, Mn = 1.11, Si = 0.29, P = 0.011, S = 0.003, Cr = 0.88, V = 0.13, Cu = 0.16 AND Mo = 0.52
Thanks a lot.
Have you used this steel or do you know which grade is or typical use?
Yes, It's look like AISI Serie 61xx, Cr-V Steel (like the legend in some handtool), but i'm not sure about the Moly content in this serie.
C = 0.22, Mn = 1.11, Si = 0.29, P = 0.011, S = 0.003, Cr = 0.88, V = 0.13, Cu = 0.16 AND Mo = 0.52
Thanks a lot.