Dear All,
We are in a big project where the sizes of pipes are very big 44", 54" and 64" with huge quantities.
Given the very tight schedule, the Contractor proposes us the use of TMCP plates for API 5L PSL2 LSAW Grade X60 welded pipes in ASME B31.3 as a process piping.
We have clearly understood the advantages and disadvantages of TMCP plates.
Knowing that the 5L API is accepted in the ASME B31.3 and the TMCP platforms have not been specified in this standards (no YES and no NO). In the 5L API, the TMCP plates are clearly cited (TMCP, Q&T, Normalized).
Can someone clarify us more so that we can decide whether or not we accept our Contractor's proposal for the use of TMCP plates for API5L PSL2 LSAW Grade X60 welded pipes in ASME B31.3 ?
Given the urgency, a prompt response is highly desirable.
Thanks in Advance
HR
We are in a big project where the sizes of pipes are very big 44", 54" and 64" with huge quantities.
Given the very tight schedule, the Contractor proposes us the use of TMCP plates for API 5L PSL2 LSAW Grade X60 welded pipes in ASME B31.3 as a process piping.
We have clearly understood the advantages and disadvantages of TMCP plates.
Knowing that the 5L API is accepted in the ASME B31.3 and the TMCP platforms have not been specified in this standards (no YES and no NO). In the 5L API, the TMCP plates are clearly cited (TMCP, Q&T, Normalized).
Can someone clarify us more so that we can decide whether or not we accept our Contractor's proposal for the use of TMCP plates for API5L PSL2 LSAW Grade X60 welded pipes in ASME B31.3 ?
Given the urgency, a prompt response is highly desirable.
Thanks in Advance
HR